7
ER316LHSi (Arcaloy 316Si/316LSi)
This wire, due to its lower carbon content, will
be less susceptible to intergranular
corrosion caused by carbide precipitation when used in place of ER316L. Again,
the higher sili- con
level (Si type) will improve the wetting, but may increase crack sensitivity if
dilution of the base material is
extensive. ER347
(Arcaloy 347) This wire is much less subject to intergranular
corrosion from carbide precipitation, as
tantalum and/or columbium are added to act as stabilizers. It is used for welding
base materials with similar
chemistry and where high temperature strength is required.